Metric Carbon U Channel


This product combination is either not available or not in stock right now. Try resetting the filters to find what you need.
Still having issues? Please Contact Us to see how we can we get you the metric metal you need.
Metric carbon U-channel here is hot-rolled European channel in S235JR and S355J2 to EN 10025, in 3 m and 6 m lengths. Two profiles are on the page, UNP and UPE, both from a nominal depth of 80 mm to 400 mm. The difference is the flange. UNP is tapered. UPE is parallel. That single fact decides whether a bolt and a flat washer sit square.
UNP and UPE
- UNP — tapered-flange channel, the traditional European U. Nominal depths on this card: 80, 100, 120, 140, 160, 180, 200, 220, 240, 260, 280, 300, 320, 350, 380, and 400. The inner face of the flange slopes, in the same spirit as an American C channel. A flat washer on the inside of a UNP flange rocks. Bolting through the flange wants a tapered washer, or a clip welded to the web, or a switch to UPE. Older European equipment drawings that say UNP mean this taper. Substituting a parallel channel changes the inside clearance and the bolt stack.
- UPE — parallel-flange channel. Nominal depths: 80, 100, 120, 140, 160, 180, 200, 220, 240, 270, 300, 330, 360, and 400. The inner faces are parallel, so a standard washer and a nut sit flat, and a plate can land between the flanges without fighting a slope. UPE is the channel to design when you are bolting a cover, a guide rail, or a bearing plate inside the U. The size steps are not the UNP steps: 270, 330, and 360 appear here, and 260, 280, 320, 350, and 380 do not.
Depth is the nominal size in the name. A UPE 200 is 200 mm deep. Flange width grows with depth and is not the same number. On the large end, a UPE 400 has a flange around 115 mm wide. Read the section for the size you are buying. The name is the depth.
S235JR or S355J2
Both grades are available on both profiles. S235JR is the everyday structural channel: minimum yield 235 MPa up to 16 mm, with 27 J impact energy at +20 °C. S355J2 raises the yield to 355 MPa in that same thickness band and moves the impact test to −20 °C. Trailer crossmembers, machine skids, and indoor frames are usually S235JR. Outdoor structures and any print that already says S355J2 should stay on that grade. Thicker webs and flanges step the minimum yield down under EN 10025-2, the same way plate does, so a UNP 400 is not designed with the thin-bar yield number.
Where channel is the section to use
Channel carries bending with the flanges in tension and compression and the web taking the shear, and it gives you a pocket. That pocket is a cable run, a belt guard, a chain guide, a door track, or a place to hide a fastener. UNP is the repair and the legacy specification, and it is the right bar when the mating part was built with the taper. UPE is the fabrication choice when new holes are going through the flange or a plate is going between the toes. For a lintel or a long span with no need for a pocket, an IPE beam is usually lighter for the same bending strength. For a wide-flange column, look at HEB. Channel is the section you pick because of the U, not because it is a small beam.
Profile, depth, grade, and length will identify a listed channel. Contact us for a depth that is not on the card or for a cut list. Sticks are 3 m and 6 m.
Frequently Asked Questions
Can I bolt through the flange of a UNP?
You can, and the washer will not sit flat on the tapered inside face. Use a tapered washer, weld a pad, or move the design to UPE, which has parallel flanges.
Is UPE 300 the same depth family as UNP 300?
Both are 300 mm deep channels, and they are different sections. Flange width, thickness, weight, and the flange slope do not match. A UPE will not drop into a UNP coping or hole pattern.
Why is there a UPE 270 and a UNP 260?
The two standards use different nominal series. UPE on this list includes 270, 330, and 360. UNP includes 260, 280, 320, 350, and 380. Order the letters and the number together.
What is the grade difference that matters in a cold building?
S355J2 is impact-tested at −20 °C. S235JR is impact-tested at +20 °C. If the channel sees winter temperatures or the drawing cites J2, order S355J2. The higher yield is part of that same grade.